50 DAFTAR PUSTAKA
Ahmed, S. and Ahsan, M. 2009. Synthesis of Ca-hydroxyapatite Bioceramic from Egg Shell and its Characterization. Bangladesh Jour Scient and Ind. Research. 43(4). pp : 501-504.
Albers, H.F. 2002. Tooth Colored Restorative Principles and Techniques : Ninth Edition. London : BC Decker Inc. pp : 44-49.
Alkhalidi, E.F., Tahlal, H., Amer A.T. 2014. Mechanical properties of New Calcium Based Cement Prepared From Egg Shell. IJERSTE. 3(3). pp : 70-72.
Anusavice, K.J., 2004, Phillips :Buku Ajar Ilmu Bahan Kedokteran Gigi. Edisi 10. Jakarta: EGC. pp : 458-460.
Apsari, A., Munadziroh, E., Yogiartono, M. 2009. Perbedaan Kebocoran Tepi Tumpatan Resin Komposit Hybrid Yang Menggunakan Sistem Bonding Total Etch Dan Self Etch. Jurnal PDGI. 3(58). pp : 1-3.
Benerjee, A. and Watson, T.F. 2014. Konservasi Restoratif, Edisi 9. Jakarta : EGC. pp: 98-99.
Beriat, N.C. and Nalbant, D. 2009. Water Absorption and HEMA Release of Resin-Modified Glass-Ionomers. Eur J Den. 3(4). pp : 267-268.
Departemen Gizi dan Kesehatan Masyarakat FKM UI, 2007. Gizi dan Startus Kesehatan . PT. Raja Gravindo Prasada. Jakarta.
Fahmi, H. and Arifin, N. 2014. Pengaruh Variasi Komposisi Komposit Resin Epoxy/Serat Glass Dan Serat Daun Nanas Terhadap Ketangguhan. Jur.Teknik Mesin. 4(2). pp : 84-85.
Karimzadeh, A., Ayatollahi, M. R., dan Shirazi, H. A. 2014. Mechanical Properties of A Dental Nano-Composite in Moist Media Determined by Nano-Scale Measurement. IJMMM. 2(1). pp : 67-68.
Karunia, D. and Spripudiyani, P. 2005. Kekuatan Geser Semen Ionomer Kaca Modifikasi sebagai Pelekat Braket Beegg Logam dengan dan Tanpa Etsa. IJD. 12(3). pp : 107-108.
51 Majedi, B. I., M. A., Mahanani, E. S., Triswari, D. 2013. Perbedaan Efektivitas Penambahan Bubuk Cangkang Telur Ayam Ras dengan Ayam Kampung Terhadap Durasi Perdarahan ( In Vivo ). IJD. 2(1). pp : 74-78.
McCabe, J.F. and Walls, A.W.G. 2015. Bahan Kedokteran Gigi, Edisi 9. Jakarta: EGC. pp: 366-377.
Moezzyzadeh, M. 2012. Evaluation of the Compressive Strength of Hybrid and Nanocomposites Introduction. Journal Dental School. 30(1). pp : 24-25.
Moshaverinia, A., Ansari, S., Moshaverinia, M., Roohpour, N., Darr, J.A., Rehman, I. 2008. Effect of incorporation of hydroxyapatite and fluoroapatite nano bioceramics into conventional glass ionomer cement (GIC). Acta biomateriaia. 4(2). pp : 432-433.
Mozartha, M., Praziandithe, M,. Sulistiawati. 2015. Pengaruh Penambahan Hidroksiapatit dari Cangkang Telur terhadap Kekuatan Tekan Glass Ionomer Cement. Jurnal B-Dent. 1(2). pp : 75-81.
Mulyawati, E., Marsetyawan., Sunarintyas S., Handajani J. 2013. Sifat fisik hidroksiapatit sintesis kalsit sebagai bahan pengisi pada sealer saluran akar resin epoxy. Dent. J. 46(4). pp : 208.
Nicholson, J.W., and Czarnecka, B. 2008. The biocompatibility of resin-modified glass-ionomer cements for dentistry. Dental Materials. 24(12). pp : 1704-1706.
Ningsih, diana setyo. 2014. Resin Modified Glass Ionomer Cement sebagai Material Alternatif Restorasi untuk Gigi Sulung. Odon Dent Jur. 1(2). pp : 46-48.
Notoatmodjo, S. 2012. Metodologi Penelitian Kesehatan. Jakarta : Rineka Cipta. pp: 50-56.
Noort, R, Van. 2007. Introduction to Dental Materials 3th ed. London: Mosby Elsevier. pp: 238-240. pp : 141-142.
Pasril, Y., and Pratama, W. A. 2013. Perbandingan Kekuatan Tekan Resin Komposit Hybrid Menggunakan Sinar Halogen Dan LED. IDJ. 2(2). pp : 84-85.
52 Pires, R.A., Fernandez, A., Nunes, T.G. 2007. Structural and Spatially Resolved Studies on the Hardening of a Commercial Resin Modified Glass Ionomer Cement. J Mater Sci : Mater Med. 18. pp : 787-788.
Purwasasmita, B.S., Ramos, S.G. 2008. Sintesis dan Karakterisasi Serbuk Hidroksiapatit Skala Sub-Mikron Menggunakan Metode Presipitasi. Jurnal Bionatural. 10(2). pp : 156-157.
Putriyanti, F., Herda, E., Soufyan, A. 2012. Strength Micro Fine Hybrid Resin Composite Yang Direndam Dalam Minuman Isotonic. Jurnal PDGI. 61(1). pp 43-44.
Powers J.M. and Sakaguchi RL. 2012.Craig’s Restorative Dental Material. 12th ed. St Louis. Mosby Co. pp: 84-181.
Powers J.M. and Wataha JC. 2008. Dental Materials Properties and Manipulation. Ed 9. Elsevier. pp: 42-49, 70-82.
Roeroe, V.M., Wicaksono, D.A., Julianti. 2015. Gambaran Kekuatann Tekan Bahan Tumpatan Semen Ionomer Kaca yang Direndam dalam Minuman Beralkohol. Jurnal e-GiGi (eG). (3)1. pp : 3-4.
Saleha., Halik, M., Annisa, N. 2015. Sintesis Dan Karakterisasi Hidroksiapatit dari Nanopartikel Kalsium Oksida ( CaO ) Cangkang Telur Untuk Aplikasi Dental Implan. Jurnal FMIPA (3). pp : 124-126.
Silva, MC., Dias, K. R. 2009. Compressive Strength of Esthetic Restorative Materials Polymerized with Quartz-Tungsten- Halogen Light and Blue LED. Braz Dent J. 20(1). pp : 54-55.
Soetojo, A. 2000. Kekuatan kompresi bahan semen glass ionomer modifikasi resin setelah perendaman dalam larutan saliva buatan. Dent J. (33). pp : 9-13.
Sonwane SR, Hambire UV. 2015. Comparison of Flexural & Compressive Strength of Nano Hybrid Composites. IJETA. 2(2). pp : 47-50.
Sosrosoedirdjo, B.I., 2004. Glass-Ionomer Modifikasi Resin.IJD. 11(1). pp : 44-45.
Sungkar, S.,Suharsini, M., Soenawan, H., 2007 . Kekuatan Geser Semen Ionomer Kaca pada Gigi Sulung setelah Aplikasi Kondisioner dengan Durasi Berbeda. IJD. 14(3). pp : 216-218.
53 Wardani, N.S., Fadli, A., Irdoni. 2015. Sintesis Hidroksiapatit dari Cangkang
Telur dengan Metode Presipitasi.JOM FTEKNIK. (2)1. pp : 1-4.